DAVID LAB
4차 산업혁명의 미래를 주도하는 미래인입니다.
Head, chin, implant, 3D printing.
Writer MERAIN
Date 22-01-17 11:36
Views 1,948

본문

1b54367a92c9d6d8150193316196e81e_1639702129_9975.jpg


We made a sample of the head width face ( chin) implant. Because the equipment currently operates cobalt chromium,


It is made of cobalt chromium. The actual production should be made of titanium.



- Process setting value.

Material: Cobalt Chrome Co-Cr (powder size 15–45 microns)

Additive thickness: 0.32 um

Laser speed: 800 m/s

Laser Capacity: 230w

Stack time: 9 hours.



1b54367a92c9d6d8150193316196e81e_1639702175_6994.jpg


This is a picture after printing and before taking it out of the build.


1b54367a92c9d6d8150193316196e81e_1639702175_0842.jpg


This is a picture of removing powder and sanding. 


The bottom is the result. Front, back. 


In general, the lattice structure has been well implemented.


1b54367a92c9d6d8150193316196e81e_1639702174_4842.jpg




1b54367a92c9d6d8150193316196e81e_1639702173_2933.jpg
1b54367a92c9d6d8150193316196e81e_1639702173_8717.jpg